Please use this identifier to cite or link to this item:
http://dspace.bits-pilani.ac.in:8080/jspui/handle/123456789/16521
Full metadata record
DC Field | Value | Language |
---|---|---|
dc.contributor.author | Panda, Sri Aurobindo | - |
dc.contributor.author | Choudhary, Sumita | - |
dc.contributor.author | Hazra, Arnab | - |
dc.contributor.author | Gangopadhyay, Subhashis | - |
dc.date.accessioned | 2024-11-28T04:49:29Z | - |
dc.date.available | 2024-11-28T04:49:29Z | - |
dc.date.issued | 2024-09 | - |
dc.identifier.uri | https://pubs.rsc.org/en/content/articlehtml/2024/ra/d4ra03128h | - |
dc.identifier.uri | http://dspace.bits-pilani.ac.in:8080/jspui/handle/123456789/16521 | - |
dc.description.abstract | Formation of highly crystalline zinc oxide (ZnO) nanowires with an extremely high aspect ratio (length = 60 μm, diameter = 50 nm) is routinely achieved by introducing an intermediate step-oxidation method during the thermal oxidation process of thin zinc (Zn) films. High-purity Zn was deposited onto clean glass substrates at room temperature using a vacuum-assisted thermal evaporation technique. Afterwards, the as-deposited Zn layers were thermally oxidized under a closed air ambient condition at different temperatures and durations. Structural, morphological, chemical, optical and electrical properties of these oxide layers were investigated using various surface characterization techniques such as X-ray diffraction (XRD), scanning electron microscopy (SEM), Raman spectroscopy, and X-ray photoemission spectroscopy (XPS). It was noticed that the initial thermal oxidation of Zn films usually starts above 400 °C. Homogeneous and lateral growth of the ZnO layer is usually preferred for oxidation at a lower temperature below 500 °C. One-dimensional (1D) asymmetric growth of ZnO started to dominate thermal oxidation above 600 °C. Highly dense 1D ZnO nanowires were specifically observed after prolonged oxidation at 600 °C for 5 hours, followed by short-step oxidation at 700 °C for 30 minutes. However, direct oxidation of Zn films at 700 °C resulted in ZnO nanorod formation. The formation of ZnO nanowires using step-oxidation is explained in terms of surface free energy and compressive stress-driven Zn adatom kinetics through the grain boundaries of laterally grown ZnO seed layers. This simple thermal oxidation process using intermittent step-oxidation was found to be quite unique and very much useful to routinely grow an array of high-density ZnO nanowires. Moreover, these ZnO nanowires showed very high sensitivity and selectivity towards formaldehyde vapour sensing against few other VOCs. | en_US |
dc.language.iso | en | en_US |
dc.publisher | RSC | en_US |
dc.subject | EEE | en_US |
dc.subject | Physics | en_US |
dc.subject | Zinc oxide (ZnO) | en_US |
dc.subject | Thermal performance | en_US |
dc.title | Surface energy and stress driven growth of extremely long and high-density ZnO nanowires using a thermal step-oxidation process | en_US |
dc.type | Article | en_US |
Appears in Collections: | Department of Electrical and Electronics Engineering |