| dc.contributor.author | Briend-Faure, Marguerite | |
| dc.contributor.author | Delafosse, Denise | |
| dc.date.accessioned | 2025-03-12T06:30:04Z | |
| dc.date.available | 2025-03-12T06:30:04Z | |
| dc.date.issued | 1977 | |
| dc.identifier.uri | http://dspace.bits-pilani.ac.in:8080/jspui/handle/123456789/18347 | |
| dc.description.abstract | The H2 reduction of Ni2+-substituted silica–magnesia gel was studied in the ranges 613–753 K and 1.3–13 kN m–2. The reaction is slow and requires an activation energy of 174 ± 20 kJ mol–1. The rate varies with the hydrogen pressure up to 6.5 kN m–2. The reduction is not complete under the experimental conditions. The mechanism of the overall reaction appears to comprise a nucleation process together with the migration of Ni2+ ions and desorption of the water formed. | en_US |
| dc.language.iso | en | en_US |
| dc.publisher | Journal of the Chemical Society : Faraday Transaction - I. The Chemical Society, London. 1977, 73 (06) | en_US |
| dc.subject | Chemistry | en_US |
| dc.subject | Kinetics | en_US |
| dc.subject | hydrogen reduction | en_US |
| dc.subject | Journal of the Chemical Society : Faraday Transaction - I | en_US |
| dc.subject | nickel ions | en_US |
| dc.subject | silica magnesia | en_US |
| dc.title | Kinetics of the hydrogen reduction of nickel ions in silica–magnesia | en_US |
| dc.type | Article | en_US |