DSpace Repository

Experimental and numerical assessment of residual stresses in aa6061 after surface treatment by deep cold rolling

Show simple item record

dc.contributor.author Kumar, Gulshan
dc.date.accessioned 2025-10-07T10:14:26Z
dc.date.available 2025-10-07T10:14:26Z
dc.date.issued 2019-10
dc.identifier.uri https://link.springer.com/chapter/10.1007/978-981-32-9072-3_9
dc.identifier.uri http://dspace.bits-pilani.ac.in:8080/jspui/handle/123456789/19654
dc.description.abstract Deep cold rolling is a mechanical method of surface treatment used to adapt the desired surface properties in machine components for aerospace industries. In this process, localized plastic deformation is rendered on the surface by rolling a form tool wheel on the specimen to condense high dislocation density which imparts high compressive residual stresses resulting in increased tensile and fatigue strength. The main focus of the present study is to characterize the distribution of residual stresses on the surface and subsurface of an 8-mm-thick plate made of an aluminium alloy AA6061-O, after deep cold rolling operation to different depths of 0.5, 1, 1.5 and 2.0 mm. The observed residual stresses are correlated with the microstructural features in the deformed depths of the specimens. The residual stress and grain size in the deformed specimens are examined by using grazing incidence X-ray diffraction and electron backscatter diffraction technique, respectively. It is observed that deep cold rolling leads to significant grain refinement, resulting in high values of residual stresses through thickness. The compressive residual stresses are found to be higher on the surface of the specimen and reduce gradually with the penetration depth. The experimental results are compared with the results obtained by FE analysis using ABAQUS. A good agreement is observed between the experimental and the simulated values of residual stresses and the trends of stress distribution pattern. en_US
dc.language.iso en en_US
dc.publisher Springer en_US
dc.subject Mechanical engineering en_US
dc.subject Deep cold rolling process en_US
dc.subject Residual stress distribution en_US
dc.subject Aluminum alloy AA6061-O en_US
dc.subject Grain refinement and finite element analysis (FEA) en_US
dc.title Experimental and numerical assessment of residual stresses in aa6061 after surface treatment by deep cold rolling en_US
dc.type Article en_US


Files in this item

Files Size Format View

There are no files associated with this item.

This item appears in the following Collection(s)

Show simple item record

Search DSpace


Advanced Search

Browse

My Account