On the characteristic length scales associated with plastic deformation in metallic glasses

dc.contributor.authorMurali, Palla
dc.date.accessioned2023-10-06T09:06:58Z
dc.date.available2023-10-06T09:06:58Z
dc.date.issued2012-05
dc.description.abstractAtomistic simulations revealed that the spatial correlations of plastic displacements in three metallic glasses, FeP, MgAl, and CuZr, follow an exponential law with a characteristic length scale ℓc that governs Poisson’s ratio ν⁠, shear band thickness tSB⁠, and fracture mode in these materials. Among the three glasses, FeP exhibits smallest ℓc⁠, thinnest tSB⁠, lowest ν⁠, and brittle fracture; CuZr exhibits largest ℓc⁠, thickest tSB⁠, highest ν⁠, and ductile fracture, while properties of MgAl lie in between those of FeP and CuZr. These findings corroborate well with existing experimental observations and suggest ℓc as a fundamental measure of the shear transformation zone size in metallic glasses.en_US
dc.identifier.urihttps://pubs.aip.org/aip/apl/article/100/20/201901/25419
dc.identifier.urihttp://dspace.bits-pilani.ac.in:8080/xmlui/handle/123456789/12243
dc.language.isoenen_US
dc.publisherAIPen_US
dc.subjectMechanical Engineeringen_US
dc.subjectMetallic Glassesen_US
dc.titleOn the characteristic length scales associated with plastic deformation in metallic glassesen_US
dc.typeArticleen_US