Fabrication of La0.7Sr0.3MnO3–Si Heterojunctions Using a CMOS-Compatible Citric Acid Etch Process
No Thumbnail Available
Date
2011-03
Authors
Journal Title
Journal ISSN
Volume Title
Publisher
IEEE
Abstract
We report La 0.7 Sr 0.3 MnO 3 (LSMO)-Si heterojunctions fabricated using a new etch process that is compatible with standard CMOS technology. For a p-n-junction device fabrication, complete etch of a masked LSMO film was done using citric acid and was confirmed using superconducting quantum interferometry device magnetometry and energy-dispersive X-ray analysis. The etch conditions were found to have a negligible effect on the step height and electrical properties of other key silicon-technology materials such as photoresists, polysilicon, and silicon dioxide. This has been confirmed using profilometer measurements and C-V characteristics.
Description
Keywords
EEE, Citric acid etch, Magnetoelectronic devices, Manganite heterojunctions, Silicon technology